Norges billigste bøker

The Microstructure of Superalloys

Om The Microstructure of Superalloys

Presenting all the main aspects of the microstructure of nickel-base superalloys, this study and includes micrographs chosen from among a large range of commercial and academic alloys, from the as-cast product to in-situ components, worn from in-service use.

Vis mer
  • Språk:
  • Engelsk
  • ISBN:
  • 9789056990978
  • Bindende:
  • Hardback
  • Sider:
  • 138
  • Utgitt:
  • 23. februar 1998
  • Dimensjoner:
  • 262x187x18 mm.
  • Vekt:
  • 404 g.
  Gratis frakt
Leveringstid: 2-4 uker
Forventet levering: 23. september 2026

Beskrivelse av The Microstructure of Superalloys

Presenting all the main aspects of the microstructure of nickel-base superalloys, this study and includes micrographs chosen from among a large range of commercial and academic alloys, from the as-cast product to in-situ components, worn from in-service use.

Brukervurderinger av The Microstructure of Superalloys



Finn lignende bøker
Boken The Microstructure of Superalloys finnes i følgende kategorier:

Gjør som tusenvis av andre bokelskere

Abonner på vårt nyhetsbrev og få rabatter og inspirasjon til din neste leseopplevelse.