Om Nanoindentation

Updated and revised, this new edition presents major advances in the theoretical understanding of nanoindentation, in an authoritative, introductory way. The book describes nanoindentation as a quantitative test method for mechanical properties of small volumes of materials.

Vis mer
  • Språk:
  • Engelsk
  • ISBN:
  • 9781441998712
  • Bindende:
  • Hardback
  • Sider:
  • 282
  • Utgitt:
  • 30. august 2011
  • Utgave:
  • 32011
  • Dimensjoner:
  • 155x235x17 mm.
  • Vekt:
  • 623 g.
  Gratis frakt
Leveringstid: 2-4 uker
Forventet levering: 4. september 2026

Beskrivelse av Nanoindentation

Updated and revised, this new edition presents major advances in the theoretical understanding of nanoindentation, in an authoritative, introductory way. The book describes nanoindentation as a quantitative test method for mechanical properties of small volumes of materials.

Brukervurderinger av Nanoindentation



Finn lignende bøker
Boken Nanoindentation finnes i følgende kategorier:

Gjør som tusenvis av andre bokelskere

Abonner på vårt nyhetsbrev og få rabatter og inspirasjon til din neste leseopplevelse.